This is the coating method to form the film by injecting the film material to the plasma flow (speed: Mach 2 and central temperature: 16,500 °C ) that is generated from the inert gas by the non-transfer arc and fused momentarily to inject the completely fused powder thermal spray materials in high speed to form the films. For the thermal spray materials, there are broad selection of metals, non-metals, ceramics (mainly the oxide and carbide), and cement, and may have the outstanding films with anti-abrasion, thermal resistance, corrosion resistance, electronic conductivity, electric cover and others, and the repairing is possible with the surface temperature of the processing for thermal spray is controlled within 150 °C that the coating is available for all materials.